Osmotic Blister Repair

Bottom of boat ‘peeledAll gel coat removed with blisters exposed

Bottom of boat ‘peeled’. All gel coat removed with blisters exposed. Old repairs are visible as brown dots.

Large blisters are ground open

Large blisters are ground open, dried and repaired with fiberglass.

Seal coat finished

Epoxy coatings under way. Seal coat finished, barrier coat is under way.

Barrier coat finished

Barrier coat finished. Ready for anti-fouling paint.

Antifouling finished ready for delivery

Antifouling finished, ready for delivery.